W. Ozgowicz et alii, Frattura ed Integrità Strutturale, 35 (2016) 11-20; DOI: 10.3221/IGF-ESIS.35.02 18 Figure 9 : The structure of industrial bronze CuSn6P in the annealed state with a grain size about 500  m after stretching (   = 1,2·10 -3 s -1 ) at the temperature: a) 150°C; b) 250°C [3]. Figure 10 : Transcrystalline mixed fracture of CuSn6P alloy after stretching at temperature of 250°C. Figure 11 : Transcrystalline mixed fracture of CuSn6P alloy after stretching at temperature of 300°C.