V. Di Cocco, Frattura ed Integrità Strutturale, 22 (2012) 31-38 ; DOI: 10.3221/IGF-ESIS.22.05 36 Tension side Compression side 15 s 60 s 180 s 360 s 900 s Figure 6 : LOM analysis of intermetallic phases damage in Zn-Ti coatings.