General Papers
On J-Dominance of Crack-Tip Fields in Largely Yielded 3D Structures | |
W. BROCKS, J. OLSCHEWSKI |
Application of Fracture Mechanics and Local Approach to Creep Crack Initiation and Growth | |
R. PIQUES, P. BENSUSSAN, A. PINEAU |
A Study of Fracture and Arrest when a Fast Propagating, Brittle Crack Emanates from a Brittle Weld into Sound 3.5% Nickel Steel | |
K. SMIT, P. BRISTOLL, Q. SYPKENS |
Characterization of Ductile Material Behaviour by J-R Curves | |
J.G. BLAUEL, B. VOSS |
Warm Prestressing of Blunt Notches | |
C.P. HARRIS, P. BOWEN, J.F. KNOTT |
Application of the Key Curve Method on Static and Dynamic J R-Curve Determination with CT— and SENB-Specimens | |
K. BRUNINGHAUS, R. TWICKLER, M. TWICKLER, A. HEUSER, D. MEMHARD, W. DAHL |
Determination of Dynamic Crack Initiation Toughness by the Instrumented Precracked Charpy Test | |
H. BLUMENAUER, R. ORTMANN |
Fracture Toughness Evaluation of a Medium Strength Al-Mg Alloy | |
J.D. DA COSTA, C.M. BRANCO, J.C. RADON |
Scatter of Fracture Toughness in the Ductile-Brittle Transition Region | |
W. EHL, D. MUNZ, A. BRÜCKNER |
Fracture Toughness Variation in a CrMoV Steel Rotor Forging at 120°C | |
S.K. BHAMBRI, G. JAYARAMAN, k. RAJANNA |
Elastic-Plastic J-Analysis for an Inner Surface Flaw in a Pressure Vessel | |
W. BROCKS, H.D. NOACK |
Calculation of Energy Release Rates for an Axissymmetric Crack Problem using the Improved Modified Crack Closure Integral Method | |
H. GREBNER, F.G. BUCHHOLZ |
Path Dependancy of the Rice J-Integral in Weld Geometries | |
M.H. BLEACKLEY, R.D. JONES, A.R. LUXMOORE |
Application of a Global-Local Blended Type Finite Element in Thermal Fracture | |
J.M. MARTINEZ ESNAOLA, I. MIRANDA, J.M. BASTERO |
J-Astry and Back to Normalcy | |
D. BROEK |
Experimental and Theoretical Determination of Leakage Areas due to Subcritical Cracks | |
G. BARTHOLOME, E. KEIM, G. SENSKI |
Fracture Analysis of a Suspension Bridge Link Eye | |
A. BLAKEBOROUGH, M. S. G. CULLIMORE, P. J. MASON |
Monotonic and Fatigue Behaviour of Rectangular Thin Walled Welded Joints used in Transport Vehicles | |
C.M. BRANCO |
Fatigue Life Assessment in Cruciform Joints | |
J. M. FERREIRA, C. M. BRANCO |
Fatigue Crack Growth in Welded Girders | |
O. I. EIDE, S. BERGE |
High Temperature Fatigue Damage Mechanisms in Alloy 800 H | |
B. KEMPF, K. BOTHE, V. GEROLD |
The Influence of Shot-Peening on The Fatigue Strength of Welded Joints in High-Strength Structural Steels | |
L. PICQUET, A. BIGNONNET, H.-P. LIEURADE |
Corrosion Fatigue Properties of an Offshore Structural Steel in Seawater Containing Hydrogen Sulphide | |
C. J. THOMAS, I. M. AUSTEN, R. BROOK, R. G. J. EDYVEAN |
The Influence of Electrochemical Parameters on the Low-Cycle Corrosion Fatigue of a Structural Steel | |
J. L. BRAZY, A. BIGNONNET, C. VALLET |
Crack Closure Effects in Fatigue Propagation of Elliptical Cracks | |
A. CLERIVET, C. BATHIAS |
The Application of J Concept to Fatigue Crack Growth in Large Scale Yielding | |
Y. Y. LAMBERT, C. BATHIAS |
Prediction of Thresholds using Cyclic Properties of Material | |
L. GUERRA ROSA, C. M. BRANCO, J. C. RADON |
The Expected Position of Fatigue Fracture Planes according to Variance of the Reduced Stress | |
W. BEDKOWSKI, E. MACHA |
Fatigue in Rate Dependent Alloy | |
Y. KATZ, A. BUSSIBA |
Fatigue Oxidation Interation in a Cr-Mo Steel | |
Z. AZARI, P. BECKER, M. LEBIENVENU, G. PLUVINAGE |
Environmental Effects on Cyclic Crack Extension | |
Y. KATZ, A. BUSSIBA |
Cleavage Fracture in a Eutectoid and Hypoeutectoid Steel | |
F. P. L. KAVISHE, T. J. BAKER |
Micromechanisms of Brittle Fracture in 2 1/4 Cr-1 Mo Weld Metal | |
P. BOWEN, M. B. D. ELLIS, M. STRANGWOOD, J. F. KNOTT |
The Effect of Non-Metallic Inclusions on Cleavage Fracture | |
T. J. BAKER, F. P. L. KAVISHE |
Mechanism of Ductile Fracture of the Low Carbon Cast Steel | |
M. BIEL |
A Study of the Ductile Tearing Mechanism during Single Overloads | |
N. RANGANATHAN, R. TINTILLER, B. BOUCHET, J. PETIT |
Sustained Load Crack Growth in an Aluminium-Silicon Bronze Alloy | |
R. D. SCHEFFEL, M. A. PHOPLONKER, J. BYRNE, R. L. JONES, P. BARNES |
Effects of Dynamic Segregation and Environment on Crack Growth at Elevated Temperature | |
P. BOWEN, C. A. HIPPSLEY, J. F. KNOTT |
The Influence of Strength and Grain Size on the Microstructural Control on Stress Corrosion Cracking of High Strength Steels | |
F. GUTIÉRREZ-SOLANA, J. GONZÁLEZ, S. BARROSO, J. M. VARONA |
Hydrogen Permeation in HSLA Steels in Relation to its Stress Corrosion Cracking Behaviour | |
F. GUTIÉRREZ-SOLANA, I. M. BERNSTEIN |
The Effect of Hydrogen on the Ductility of Aluminium-Tin Alloys | |
A. K. BUSBY,, J. W. MARTIN |
Numerical Treatment of Fracture Mechanics Problems | |
V. Z. PARTON, V. G. BORISKOVSKY |